![a-cheaper-way-to-scale-up-atomic-layer-deposition](https://utterbuzz.com/wp-content/uploads/2019/11/a-cheaper-way-to-scale-up-atomic-layer-deposition-640x905.jpg)
Chemical engineers have developed a new method for atomic layer deposition, a technique commonly used in high-quality microelectronics. The new method can be used in materials with larger surfaces much more cheaply than current approaches, while preserving quality and efficiency.